{"id":297275,"date":"2024-10-19T20:14:24","date_gmt":"2024-10-19T20:14:24","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/astm-d6442-2020\/"},"modified":"2024-10-25T17:34:12","modified_gmt":"2024-10-25T17:34:12","slug":"astm-d6442-2020","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/astm\/astm-d6442-2020\/","title":{"rendered":"ASTM-D6442 2020"},"content":{"rendered":"

ASTM D6442-06-Reapproved2020<\/h3>\n

Active Standard: Standard Test Method for Determination of Copper Release Rate From Antifouling Coatings in Substitute Ocean Water<\/h4>\n
\n

ASTM D6442<\/h4>\n

Scope<\/strong><\/p>\n

\n

1.1<\/span> This test method covers the laboratory determination of the rate at which copper is released from an antifouling (AF) coating in substitute ocean water. The practical limits for quantifying copper release rates by this method are from 1.8 to 500 \u03bcg cm-2<\/sup>d-1<\/sup>. This range may be extended to 0.2 to 500 \u03bcg cm-2<\/sup>d-1<\/sup> if the analytical procedure described in Appendix X1<\/span> is followed.<\/p>\n

\n

Note 1:<\/span> The term \u201csubstitute ocean water\u201d is used throughout this standard to refer to artificial or synthetic seawater prepared in accordance with Practice D1141<\/span>.<\/span><\/p>\n<\/p><\/div>\n<\/p><\/div>\n

\n

1.2<\/span> The procedure contains the preparation steps for the release rate determination of copper from antifouling paints including apparatus, reagents, holding tank conditions, and sampling point details. Analysis for the concentration of copper in substitute ocean water requires the accurate determination of copper at the low parts \u03bcg L-1<\/sup> (parts per billion, ppb) level. To detect and correct for reagent impurities, acceptable analytical precision standards are necessary. Therefore, the limit of quantitation (LOQ) for copper in substitute ocean water for the analytical method shall be 10 \u03bcg L-1<\/sup> (10 ppb) or less. The procedure for determining the LOQ for copper in substitute ocean water for the analytical method is found in Annex A2<\/span>.<\/p>\n<\/p><\/div>\n

\n

1.3<\/span> A suitable method is described in Appendix X1<\/span> (graphite furnace atomic absorption spectroscopy, GF-AAS). Other analytical methods may be utilized with relevant procedural changes, as needed, to accommodate selected specific methods. Such methods must meet the limit of quantitation for copper in substitute ocean water of 10 \u03bcg L-1<\/sup>\u2007(10 ppb) or less. See 1.2<\/span>.<\/p>\n<\/p><\/div>\n

\n

1.4<\/span> This results of this test method do not reflect environmental copper release rates for antifouling products, and are not suitable for direct use in the process of generating environmental risk assessments, environmental loading estimates, or for establishing release rate limits for regulatory purposes. See also Section 4<\/span> on Significance and Use.<\/p>\n<\/p><\/div>\n

\n

1.5<\/span> The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.<\/p>\n<\/p><\/div>\n

\n

1.6<\/span> This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. For specific hazard statements, see Section 7<\/span>.<\/span><\/i><\/p>\n<\/p><\/div>\n

\n

1.7<\/span> This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.<\/i><\/p>\n<\/p><\/div>\n

Keywords<\/strong><\/p>\n

antifouling coating; copper; release rate;<\/p>\n

ICS Code<\/strong><\/p>\n

ICS Number Code 87.040 (Paints and varnishes)<\/p>\n

DOI:<\/strong> 10.1520\/D6442-06R20<\/p>\n<\/div>\n","protected":false},"excerpt":{"rendered":"

D6442-06(2020) Standard Test Method for Determination of Copper Release Rate From Antifouling Coatings in Substitute Ocean Water<\/b><\/p>\n\n\n\n\n
Published By<\/td>\nPublication Date<\/td>\nNumber of Pages<\/td>\n<\/tr>\n
ASTM<\/b><\/a><\/td>\n2020<\/td>\n10<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n","protected":false},"featured_media":297279,"template":"","meta":{"rank_math_lock_modified_date":false,"ep_exclude_from_search":false},"product_cat":[2637],"product_tag":[],"class_list":{"0":"post-297275","1":"product","2":"type-product","3":"status-publish","4":"has-post-thumbnail","6":"product_cat-astm","8":"first","9":"instock","10":"sold-individually","11":"shipping-taxable","12":"purchasable","13":"product-type-simple"},"_links":{"self":[{"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/product\/297275","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/product"}],"about":[{"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/types\/product"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/media\/297279"}],"wp:attachment":[{"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/media?parent=297275"}],"wp:term":[{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/product_cat?post=297275"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/pdfstandards.shop\/wp-json\/wp\/v2\/product_tag?post=297275"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}