ASTM-A608 2006
$40.63
A608/A608M-06 Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperature
Published By | Publication Date | Number of Pages |
ASTM | 2006 | 6 |
1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.
1.2 The grades of high alloys detailed in are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.
1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.
1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of each other. Combining values from the two systems may result in nonconformance with the specification.
PDF Catalog
PDF Pages | PDF Title |
---|---|
1 | Scope Referenced Documents Ordering Information |
2 | General Requirements Materials and Manufacture Chemical Requirements Tensile Properties Permissible Variation in Dimensions TABLE 1 TABLE 2 |
3 | Finish Pressure Test Flattening Test Mechanical Tests Required Certification Product Marking Keywords TABLE 3 TABLE 4 |
4 | TABLE S2 |
5 | TABLE S3 |