BS 6057-1.2:1990

$86.31

Rubber latices. Specification and coding – Specification for evaporated, preserved natural rubber latices

Published By Publication Date Number of Pages
BSI 1990 8
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

This International Standard gives specifications for natural rubber latex concentrate which has been concentrated by evaporation. It does not apply to natural rubber latex concentrates which have been concentrated by centrifuging or creaming, or to latices from natural sources other than Hevea brasiliensis, or to compounded latex or vulcanized latex.

This International Standard covers requirements for evaporated natural rubber latex concentrates of the following types:

NR latex, type HA evaporated: Evaporated latex concentrate preserved with ammonia only or with ammonia together with other preservative(s), with an alkalinity of at least 0,60 % (m/m) with respect to the latex.

NR latex, type KHS evaporated: Evaporated latex concentrate preserved with potassium hydroxide and having a nominal total solids content of 73 % (m/m).

NR latex, type KLS evaporated: Evaporated latex concentrate preserved with potassium hydroxide and having a nominal total solids content of 68 % (m/m).