$25.35

Automotive Austempered Ductile (Nodular) Iron Castings (ADI)

Published By Publication Date Number of Pages
SAE 2018-01-09 13
Guaranteed Safe Checkout
Categories: , ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

This SAE Standard covers the mechanical and physical property requirements for Austempered Ductile Iron (ADI) castings used in automotive and allied industries. Specifically covered are:
  1. a

    Hardness
  2. b

    Tensile Strength
  3. c

    Yield Strength
  4. d

    Elongation
  5. e

    Modulus of Elasticity
  6. f

    Impact Energy
  7. g

    Microstructure
In this document SI units are primary and in-lb units are derived. Appendix A provides general information and related resources on the microstructural, chemical and heat treatment requirements to meet the mechanical properties needed for ADI in particular service conditions and applications.