INTRODUCTION

Intent

This procedure is used to measure the retention characteristics
of the resilient member of a fiber optic component (most commonly a
connector). It is specifically intended for use when it is
impracticable to define acceptance/rejection criteria for resilient
members by the use of size dimensions.

Description

The method is applicable to either male or female resilient
members. For the case of a male member, a ring gauge is forced over
the member and the minimum frictional force to pull it off is
assessed by its ability to pick up a weight. The procedure is
identical for a female resilient member except that a gauge pin is
substituted for the ring gauge.

Alternative Procedures

This test procedure is an alternative to the measurement
procedure, titled Gauge Retention Force, of IEC 874-1, Third
Edition.