{"id":420373,"date":"2024-10-20T06:30:48","date_gmt":"2024-10-20T06:30:48","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/bs-en-iec-60404-132018-3\/"},"modified":"2024-10-26T12:11:01","modified_gmt":"2024-10-26T12:11:01","slug":"bs-en-iec-60404-132018-3","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/bsi\/bs-en-iec-60404-132018-3\/","title":{"rendered":"BS EN IEC 60404-13:2018"},"content":{"rendered":"
This part of IEC 60404 specifies the methods used for determining the resistivity, density and stacking factor of grain-oriented and non-oriented electrical steel strip and sheet. These quantities are necessary to establish the physical characteristics of the material. Moreover, the density is necessary to allow specified values of the magnetic polarization, resistivity and stacking factor to be determined.<\/p>\n
Since these properties are functions of temperature, the measurements will be made at an ambient temperature of (23 \u00b15) \u00b0C except when specified in this document.<\/p>\n
PDF Pages<\/th>\n | PDF Title<\/th>\n<\/tr>\n | ||||||
---|---|---|---|---|---|---|---|
2<\/td>\n | undefined <\/td>\n<\/tr>\n | ||||||
5<\/td>\n | Annex ZA(normative)Normative references to international publicationswith their corresponding European publications <\/td>\n<\/tr>\n | ||||||
7<\/td>\n | English CONTENTS <\/td>\n<\/tr>\n | ||||||
9<\/td>\n | FOREWORD <\/td>\n<\/tr>\n | ||||||
11<\/td>\n | 1 Scope 2 Normative references 3 Terms and definitions <\/td>\n<\/tr>\n | ||||||
12<\/td>\n | 4 Determination of the resistivity 4.1 General 4.2 Principles of measurement 4.2.1 Method of determining \u03c1 for an Epstein strip specimen (Method R1) Figures Figure 1 \u2013 Circuit for the measurement of resistance ofan Epstein strip specimen (Method R1) <\/td>\n<\/tr>\n | ||||||
13<\/td>\n | 4.2.2 Method of determining \u03c1 for a rectangular sheet specimen (Method R2) with supplementary remarks for strip specimen Figure 2 \u2013 Circuit for the measurement of resistance ofa rectangular sheet specimen (Method R2) <\/td>\n<\/tr>\n | ||||||
14<\/td>\n | 4.2.3 Determination of thickness d <\/td>\n<\/tr>\n | ||||||
15<\/td>\n | 4.3 Test specimen 4.3.1 Epstein strip specimen 4.3.2 Rectangular sheet specimen 4.4 Apparatus 4.4.1 Common requirements for Method R1 and Method R2 4.4.2 Requirements for Method R1 <\/td>\n<\/tr>\n | ||||||
16<\/td>\n | 4.4.3 Requirements for Method R2 4.5 Measuring procedure 4.5.1 Determination of the thickness d of the test specimen 4.5.2 Procedure with strip specimen (Method R1) 4.5.3 Procedure with rectangular sheet specimen (Method R2) 4.6 Reproducibility <\/td>\n<\/tr>\n | ||||||
17<\/td>\n | 4.7 Test report 5 Determination of the density 5.1 General <\/td>\n<\/tr>\n | ||||||
18<\/td>\n | 5.2 Method based on the measurement of resistance (Method D1) 5.2.1 Principles of measurement Figure 3 \u2013 Experimental data and the regression line of the density \u03c1m againstthe product \u03c1m\u00b7\u03c1 for non-oriented electrical steel sheet [6] <\/td>\n<\/tr>\n | ||||||
19<\/td>\n | 5.2.2 Test specimen 5.2.3 Measuring procedure <\/td>\n<\/tr>\n | ||||||
20<\/td>\n | 5.2.4 Reproducibility 5.3 Gas pyknometer method (Method D2) 5.3.1 Principles of measurement 5.3.2 Test specimen 5.3.3 Test apparatus 5.3.4 Measuring procedure 5.3.5 Reproducibility 5.4 Test report <\/td>\n<\/tr>\n | ||||||
21<\/td>\n | 6 Determination of the stacking factor 6.1 General 6.2 Test specimen 6.3 Measuring procedure <\/td>\n<\/tr>\n | ||||||
22<\/td>\n | 6.4 Reproducibility 6.5 Test report Figure 4 \u2013 Schematic diagram of stacking specimen and rams <\/td>\n<\/tr>\n | ||||||
24<\/td>\n | Annex A (informative)An example of the apparatus for the measurement of the resistivityusing a rectangular sheet specimen (Method R2) Figure A.1 \u2013 Schematic cross-sectional view of the arrangementof the contact holder <\/td>\n<\/tr>\n | ||||||
25<\/td>\n | Annex B (informative)An example of the determination of density usingthe gas pyknometer method (Method D2) B.1 Overview B.2 Test specimen Table B.1 \u2013 Number of test discs of diameter 36 mm <\/td>\n<\/tr>\n | ||||||
26<\/td>\n | B.3 Apparatus B.4 Calibration B.5 Measuring procedure Figure B.1 \u2013 Diagram illustrating the two-chamber pressure gas pyknometer <\/td>\n<\/tr>\n | ||||||
27<\/td>\n | B.6 Repeatability <\/td>\n<\/tr>\n | ||||||
28<\/td>\n | Annex C (informative)Calculation of density based onsilicon and aluminium content (Method D4) <\/td>\n<\/tr>\n | ||||||